BALL MILL CRACK REPAIR

BALL MILL CRACK REPAIR

ANALYSIS

EQUIPMENT
BALL MILL

COMPONENT NAME
MATERIAL FIDDEN INLET PLATE

TYPE OF PROBLEM
JOINING/CRACK

PROBLEM DUE TO
HEAVY WEIGHT/LOAD BEARING SERVICE CONDITION

BASE METAL
C-0.12-0.2%, SI<0.3, MN-<0.7, SULPHUR<0.45%, PH<0.45%.

DIMENSION (M.M) T
85

DIMENSION (M.M) Dia
36 BOLTS, EACH HEAVING DIA OF 60

Procedure

1. BOTH SIDES OF THE PLATE WERE GROUND TO V GROOVE.

2. ALIGNMENT WAS DONE.

3. WELDING ROOT RUN WITH 3.15DIA ELECTRODE & THEN COMPLETED THE JOB WITH 4.0MM DIA ELECTRODES.

4. FINALLY DP TEST IS DONE