GEAR TEETH REBUILDING

Industry Type

Product Group

Our solution

Product
LOTHERME 468

Size (mm)
4.00

Current (AMPs)
100-150

Qty. (Kgs)
4

JOB PICTURES

None

None

ANALYSIS

COMPONENT NAME
DRIVE GEAR

TYPE OF PROBLEM
TEETH BROKEN

PROBLEM DUE TO
LOAD & IMPACT

PREVIOUS SOLUTION
EUT 680CGS

BASE METAL
EN 18

Procedure

1. INSPECTION & CLEANING OF THE JOB.

2. DRILLED HOLES & INSERTED THE STUDS

3. GRINDED OUT TO REMOVE UNWANTED BURS

4. STARTED REBUILDING USING LOTHERME 468

5. FINAL GRINDING CARRIED OUT.


LoTherme-468 filler wire and flux material are so chosen that it is highly favorable for producing welds which have complete freedom from hazards of cracking on a wide variety of similar and dissimilar steels.