MSF Shaft Reconditioning In Furnace

Industry Type
Steel

Product Group
Lotherme

OUR SOLUTION

Problem
Wear

Dimensions & Weight
3000L x 200Dia

Previous Solution
Overlaying

Our Product Used
LothermeGS 602

Size (mm)
2.4mm

Quantity (Kgs)
40

ANALYSIS

Equipment Name
Furnace

Base Metal
15Mo3

Material Handled
Molten Iron

Temp (Deg.C)
750-800

Wear Factor
Temp, Abrasion

JOB PICTURES

Job Pic Before Repair

Job Pic Before Repair

Job Pic After Repair

Job Pic After Repair

Procedure

-Clean area of shaft surface and removing hook from shaft as mentioned in below picture.

-Pre heat the job 250deg before welding

-Follow GMAW process using Our Product LoTherme GS602 and maintain inerpass temp.

-Build up on shaft to its original dimension

-Slow cooling required after welding.

-Machining