Industry Type
Steel Foundry
Product Group
Lotherme
OUR SOLUTION
Problem
Pin & Blow Hole
Dimensions & Weight
L-5500 mm xT- 225 mm x W-450 mm & WT- 1080 kgs
Previous Solution
Ok 13MN (esab)
Our Product Used
L-607
Size (mm)
4.00
Quantity (Kgs)
½ kgs approx
ANALYSIS
Equipment Name
Crossing
Base Metal
Mn Steel
Wear Factor
Buildup finishing
JOB PICTURES
Job Pic Before Repair
Job Pic After Repair
Procedure
Dry electrodes at 2500C for one hour. clean the weld area very well by gauging, grinding and cleaning agent after that DP test done due to fully remove the crack from the metal, then use our L-607 with low current ,shot arc and stringer beads for joining or resurfacing of austenitic mn steel.